It can be used to the corrosion resistance of stainless steel structure, such as the 06Cr19Ni9 and 06Cr19Ni11Ti, whose working temperature below 300 ℃; it can also be used for stainless steel structure using under cryogenic temperatures, such as liquid nitrogen container, liquefied natural gas containers, etc.


Product Detail

Product Category

Product Tags

The organization keeps for the procedure concept “scientific administration, superior quality and effectiveness primacy, shopper supreme for Quality Inspection for China Welding Construction Welding Work Steel Structure and Steel Manufacturing Weldments Through Arc Welding, We sincerely do our best to offer the best service for all the clients and businessmen.
The organization keeps for the procedure concept “scientific administration, superior quality and effectiveness primacy, shopper supreme for China OEM Welding Parts, Welding of Large Carbon Steel Structural Parts, Our company has already had a lot of top factories and experienced technology teams in China, offering the best products, techniques and services to worldwide customers. Honesty is our principle, qualified operation is our work, service is our goal, and customers’ satisfaction is our future!
APPLICATIONS:

It can be used to the corrosion resistance of stainless steel structure, such as the 06Cr19Ni9 and 06Cr19Ni11Ti, whose working temperature below 300 ℃; it can also be used for stainless steel structure using under cryogenic temperatures, such as liquid nitrogen container, liquefied natural gas containers, etc.

CHARACTERISTICS:

E308-16 is a coated rutile type Cr18Ni9 stainless steel. Both AC and DC can be used and can be all-position welding. It can reach excellent welding performance, stable arc, little spatter, easy slag removal and good weld appearance. The deposited metal has good resistance to inter granular corrosion.

ATTENTION:

1. The electrodes must be baked by 320-350 ℃ for 1 hour before welding, dry the electrode when use it.

2. The rust, oil, water and other impurities of the weld must be removed before welding.

3.Recommended DC power supply, because AC welding has a shallow penetration, the current should not be too large, in order to avoid the coating redness and cracking.

4. To minimize the amount of heat input and welding electrode oscillating amplitude should not be too big.

5. Preheat and interlayer-temperature should remain below 150 ℃

WELDING POSITIONS:

PA, PB, PD, PF

DEPOSIT COMPOSITION (Quality Score):  %

items

C

Cr

Ni

Mo

Mn

Si

P

S

Cu

Requirements

≤0.08

18.0-21.0

9.0-11.0

≤0.75

0.5-2.5

≤1.00

≤0.04

≤0.03

≤0.75

Typical Results

0.062

19.34

10.14

0.28

1.08

0.66

0.025

0.010

0.08

MECHANICAL PROPERTIES:

items

Tensile Strength

Rm/MPa

Elongation A/%

Charpy V-Notch

KV2(J)-196℃

Requirements

≥550

≥30

≥29

Typical Results

570

38

36

TYPICAL OPERATING PROCEDURES: (AC, DC+)

Diameter (mm)

2.0

2.5

3.2

4.0

5.0

Current (A)

25-50

50-80

80-110

110-160

160-200

PACKAGING:

5kg/box, 4boxes/carton, 20kgs/carton, 50cartons/pallet. 21MT -26MT per 1X20″ FCL.

OEM/ODM:

We support OEM/ODM and could make packaging accord to your design, please contact us for detail discussion.

General requirements:
The manufacture of welded structural parts shall comply with the design, process documents and the provisions of this standard. 3.2 Requirements for ambient temperature during welding production:
When parts and finished products are rectified, the temperature should not be lower than the following:
Low carbon steel material: -20℃;
Low alloy structural steel material: -15℃.
Generally, the allowable welding temperature of welding parts should meet the requirements of Table.
When welding parts are welded under low temperature conditions (as listed in Table 1), the surface of the steel should be preheated. The width of the preheating zone must be greater than 4 times the thickness of the plate to be welded, and the preheating width on each side must not be less than 100mm. Welding can only be done after heating to 100~~200℃. If flame preheating is used, the distance between the flame core and the board surface should be greater than 50mm.
Under normal temperature conditions, for welding parts with high rigidity and poor weldability, preheating should also be carried out before welding (the preheating temperature is within the range of 100~200℃), and heat preservation or tempering should be carried out after welding to eliminate welding stress.

 The organization keeps for the procedure concept “scientific administration, superior quality and effectiveness primacy, shopper supreme for Quality Inspection for China Welding Construction Welding Work Steel Structure and Steel Manufacturing Weldments Through Arc Welding, We sincerely do our best to offer the best service for all the clients and businessmen.
Quality Inspection for China OEM Welding Parts, Welding of Large Carbon Steel Structural Parts, Our company has already had a lot of top factories and experienced technology teams in China, offering the best products, techniques and services to worldwide customers. Honesty is our principle, qualified operation is our work, service is our goal, and customers’ satisfaction is our future!


  • Previous:
  • Next:

  • Send your message to us:

    Write your message here and send it to us

    Related Products

    Send your message to us: